SOLIBOND C PLUS COBALT-CHROME ALLOY
Nickel- and beryllium-free chrome-cobalt alloy. Very fine oxide layer. Excellent flowability ensures stable casting results. Shines and polishes quickly. Optimal bonding to ceramics. Composition: Co 63%, Cr 24%, Mo 2.9%, W 1%, Nb 0.9%, Si 1.1% Melting range: 1310-1370ºC. Casting temperature: 1430ºC. Vickers hardness: 280HV. Elongation at break: 10.1%. CTE (20–600°C): 14.0 (x10-6/K) CTE (25–500°C): 13.9 (x10-6/K)