-15%
SOLIBOND N NICKEL-CHROME ALLOY
Excellent flowability ensures stable casting results. Outstanding accuracy with a low hardness. Very fine oxide layer and optimal bonding to ceramics. Composition: Ni 62.7%, Cr 24.5%, Mo 10.4%, Si 1.4%, Fe 1.0% Melting range: 1250–1330°C. Casting temperature: 1390°C. Vickers hardness: 180HV. Elongation at break: 25.0%. CTE (20–600°C): 14.1 (x10-6/K) CTE (25–500°C): 13.9 (x10-6/K)